Chemical Foaming Agent | |||||
Name | Application | Type | Decomposition TemperatureºC | Gas evolution [m/g(STP)] |
Average partide size(um) |
High temperature AC foaming agent |
Plastic, rubber foaming |
AC-6(AC 1000) DG-04 |
200~208 | ≥220 | 4~6 |
(AC 3000) DG-03 |
200 | ≥220 | 9~10 | ||
(AC 7000) DG-07 |
200 | ≥220 | 3~5 | ||
Normal AC foaming agent |
Plastic, rubber foaming. The foaming of EVA, MD in big or small mould. |
AD-6 | 150~200 | 190~200 | 8~10 |
AD-8 | 150~180 | 190~195 | 8~10 | ||
AD-10 | 160~180 | 180~190 | 8~10 | ||
AD-11 | 160~200 | 180+5 | 8~10 | ||
Artificial leather foaming agent |
PVC artificial leather and half PU artificial leather |
ACR-8 | 200+5 | ≥220 | 6~8 |
ACR-10 | 170+5 | ≥200 | 5~7 | ||
The series of DG white foaming agent |
TPR,PVC gas injection foaming process |
DG-1 | 140~170 | ≥110 | 5~6 |
DG-4 | 140~170 | ≥90 | 5~6 | ||
DG-5 | 140~170 | ≥130 | 5~6 | ||
AC-6T foaming agent |
The injection foaming process of PVC,TPR,PS profiles, sheets, plates Plastic, rubber foaming. PVC, PE, PP tube foaming, foam layer of leather foaming. |
AC-6T1# | 160~180 | 170+5 | 6~8 |
AC-6T2# | 140~180 | 170+5 | 6~8 | ||
AC-6T3# | 150~180 | 150+5 | 6~8 | ||
AC-6T4# | 150~170 | 145+5 | 6~8 | ||
AC-135 | 135+2 | 160+5 | 7~8 | ||
AC-165 | 165+2 | 180+5 | 8~10 | ||
AK-8 | 125~160 | 130+5 | 7~8 | ||
Injection foaming agent |
EVA injection foaming process |
AC-3000H1# | 188+5 | ≥185 | 5~10 |
AC-3000H2# | 180+2 | ≥190 | 5~10 | ||
AC-6000H1# | 180+2 | ≥170 | 5~10 | ||
AC-6000H2# | 170~178 | ≥180 | 5~10 | ||
Physical Foaming Agent | |||||
Name | Application | Type | Start Expansion TemperatureºC | Maximum Expansion TemperatureºC | Average partide size(um) |
Physical Expandable Microsphere | TPR,PVC gas injection foaming process,EVA injection foaming process,Plastic, rubber foaming | ADVANCELL WS606 | 140-150ºC | 180-190ºC | 26~34 |